http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013071255-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-40 |
filingDate | 2011-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8bfc20b173ffc2ac694947576349bfe5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f4a86dafaa63dd20b783e4b3db71e589 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_26f7e04a5f48192d30743278a3181ee2 |
publicationDate | 2013-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013071255-A |
titleOfInvention | Three-dimensional decorative film, decorative molded product with base material, decorative molded product, and methods for producing the same |
abstract | [PROBLEMS] To provide a three-dimensional decorative film for use in an injection molding simultaneous transfer decorative method for imparting design properties to a decorative resin molded product, having a good primer printing surface and excellent drying properties. Three-dimensional molding decoration that does not deteriorate the transferability of the decorative layer, has good moldability (shape followability), and has good initial adhesion between the decorative layer and the protective layer and good adhesion after the heat test. Provision of film. A three-dimensional decorative film is formed by laminating a release layer 12, a protective layer 13, a primer layer 14, and a decorative layer 15 in this order on a substrate 11, and the protective layer is ionized. A cured product of a radiation curable resin composition, the primer layer is a cured product of a primer composition containing a polyol and an isocyanate, and the glass transition temperature Tg of the polyol is 55 ° C. or higher; and A hydroxyl value is 30 to 130 mgKOH / g, a three-dimensional molded decorative film, a decorative molded product using the same, and a method for producing them. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020163865-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017110780-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017186500-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11529798-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017065244-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7291655-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017051539-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10792903-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021154706-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6015877-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016002692-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016072450-A1 |
priorityDate | 2011-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 146.