Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d826a0e6b3def82ac3e34b9caaf74b75 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_96ec3985e3ce9b24614fb87bf51a4f12 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25B11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25B11-031 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25B1-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-8621 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-8652 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25B9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25B11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25B11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-02 |
filingDate |
2012-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7aeb6dec9b6afdfe51968f212cfcc95c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dbf6d95542a0108b32aafd322d8cf69b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3f00adec8a7146927685af216b4ca96a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4efaad02753300eb0c56ebed83637779 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e2361cab882107fb01541c37c8d17aec |
publicationDate |
2013-04-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2013067861-A |
titleOfInvention |
Oxygen consuming electrode and method for producing the same |
abstract |
An oxygen consuming electrode in which silver oxide is used, in particular for use in chlor-alkali electrolysis, in which the disadvantages of the prior art are eliminated, and a low operating voltage in chlor-alkali electrolysis, and a method for producing the same provide. A) A sodium hydroxide aqueous solution and a silver nitrate solution are simultaneously added to a receiver while maintaining a pH constant within a range of 10 to 12 and maintaining a temperature within a range of 20 to 80 ° C. A step of precipitating silver oxide by using a mechanical stirrer to introduce stirring energy in the range of 0.01-10 W / L, b) a step of removing the precipitated silver oxide of step a) from the suspension, c) D) drying the silver oxide at a temperature in the range of 80 to 200 ° C. under reduced pressure and optionally in an inert gas atmosphere, d) the obtained silver oxide is converted into a conductive support material, a silver particle-containing catalyst and a fine powder fluorinated A method for producing an oxygen consuming electrode, comprising a step of further processing together with a polymer to form a planar oxygen consuming electrode. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101556342-B1 |
priorityDate |
2011-09-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |