http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013064100-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G61-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-22 |
filingDate | 2012-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f46700873f7ac96a4b79b041d5d8102f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e9f0f3678fc0d36dc6dc9f786ffc8d3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bf339f9dc49281566d98d8db192623d9 |
publicationDate | 2013-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013064100-A |
titleOfInvention | Method for producing thin film comprising sulfo group-containing polymer as constituent and method for obtaining sulfo group-containing polymer |
abstract | [PROBLEMS] To obtain a thin film production method and a polymer which are advantageous in industrial production, with the effects of improving production speed, reducing costs by reducing the number of processes, and reducing the amount of acid used for reducing the amount of acid waste. Providing a method. A method for producing a thin film comprising a sulfo group-containing polymer having an ion exchange capacity of 0.5 to 8.5 meq / g by a titration method as a constituent component, wherein the formula (1-1) R 0 possessed by the poorly water-soluble polymer having a group represented by the formula is eliminated in the presence of water at a reaction temperature of 90 to 200 ° C. in the absence of a Bronsted acid or the like having an acid dissociation constant <10. From the step, the step of recovering the produced sulfo group-containing polymer without isolating it as a solid, the step of applying the recovered sulfo group-containing polymer on a substrate in a liquid state, and the obtained coated product A method comprising a step of forming a thin film containing the sulfo group-containing polymer as a constituent component on a substrate by removing a liquid. [Selection figure] None |
priorityDate | 2011-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |