http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013058793-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_063a1b324005ddc15e16e7529c6258c4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-04 |
filingDate | 2012-11-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5888a69f2200598d89776c135d02eeac http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_88e2801cde1999bd9aa0cfa20ec1824e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1b73eea050d6f76d65bdaacbef96a88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_adb793a22012d0514ca63f3fb8755e64 |
publicationDate | 2013-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013058793-A |
titleOfInvention | Solid electrolytic capacitor |
abstract | An object of the present invention is to provide a solid electrolytic capacitor having a small change in ESR with time even under a high temperature environment, and a method for manufacturing the same. An anode body 11 made of a valve metal, a dielectric oxide film layer 12 formed on the surface of the anode body 11, and a solid electrolyte layer 13 formed on the surface of the dielectric oxide film layer 12. In the solid electrolytic capacitor having the capacitor element 15 composed of the carbon layer 14a and the conductor layer 14b sequentially formed as the cathode layer 14 on the surface of the solid electrolyte layer 13, the carbon layer 14a is condensed with aromatic sulfonic acid formaldehyde. Product, polystyrene sulfonic acid, or a solid electrolytic capacitor comprising at least one of these salts. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021172123-A1 |
priorityDate | 2007-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 70.