http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013049825-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a696e8ab693ab78a931db09817fad566 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61Q19-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-81 |
filingDate | 2012-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9444a7e7104bd290569df1bbe78022d5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50bc5e7d8a1d2b3cde5a5695a4fea8c1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_847f36c6274fe18df77ac010c751b56c |
publicationDate | 2013-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013049825-A |
titleOfInvention | Oval shaped resin particles, production method thereof, and use thereof |
abstract | An object of the present invention is to provide a novel shaped irregular shaped resin particle capable of improving characteristics such as light diffusibility, adhesion and oil absorption, a production method thereof, and use thereof. The deformed resin particles include a resin layer 1 forming a surface layer of the deformed resin particles, and a deformed resin including a resin core 2 formed of a resin component different from the resin layer 1 and formed inside the resin layer 1. A particle having a single depression 3 and the resin core 2 having an ellipsoidal shape and adjacent to the depression 3, the ratio of the minor axis B of the irregular resin particle to the major axis A of the irregular resin particle B / A is 0.7 or more. The method for producing the irregular shaped resin particles includes a first step of producing resin particles by polymerizing a fluorine-containing (meth) acrylic acid ester monomer containing 0.1 to 5% by mass of a polyfunctional monomer. The second step of polymerizing the resin particles obtained in the first step after absorbing the (meth) acrylic acid ester monomer containing 1 to 50% by mass of the polyfunctional monomer; Is included. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019147967-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016222897-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021014592-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11078314-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2018179687-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7277425-B2 |
priorityDate | 2011-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 86.