http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013049824-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_06ea9f956e87fb918ac61ef4acb5b2be |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 |
filingDate | 2011-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4510afe411b1b30960a07a652cd07fe5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9fe468dc3fe88343d6f949b25a540c3e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_885043651eea539a2f6eab989fff1811 |
publicationDate | 2013-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013049824-A |
titleOfInvention | Graft copolymer and thermoplastic resin composition |
abstract | 【Task】 To provide a graft copolymer excellent in impact resistance and fluidity using a rubbery polymer excellent in polymerization stability, a thermoplastic resin composition obtained from the graft copolymer, and a molded product thereof. [Solution] 5 to 80 parts by weight of rubbery polymer, at least one monomer selected from aromatic vinyl monomers, vinyl cyanide monomers and other vinyl monomers copolymerizable therewith A graft copolymer obtained by graft polymerization of 20 to 95 parts by weight of a polymer, wherein the rubbery polymer has a microstructure of 21 to 30% of cis-1,4 bonds and 47 of trans-1,4 bonds. A graft copolymer, characterized in that -60%, 1,2 vinyl bond is 16-23%, and the degree of swelling of the rubbery polymer is 13-35. [Selection figure] None |
priorityDate | 2011-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |