Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2403-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-417 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-451 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-449 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-446 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-491 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-489 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-0427 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-043 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-403 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-4295 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-429 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-043 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-451 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B38-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-491 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-417 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-429 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-403 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-489 |
filingDate |
2012-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1cb66e6cdd523c0c016c33e2cf15c421 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_032339c46e15e6913e4962ca5d5e59fd |
publicationDate |
2013-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2013046901-A |
titleOfInvention |
Method for producing laminated porous film |
abstract |
A method for producing a laminated porous film having a substrate porous film and a heat-resistant layer is provided. [Solution] A coating slurry containing a solvent, a binder resin and a filler is applied to the surface of the substrate porous film, and then the solvent is removed to form a heat-resistant layer mainly composed of a filler on the surface of the substrate porous film. Wherein the coating slurry is prepared so that a contact angle with respect to the untreated porous substrate film is 75 ° or more, and the coating slurry is further applied to the surface of the porous substrate film. Before applying the coating slurry, surface treatment of the substrate porous film is performed so that the contact angle of the coating slurry with respect to the substrate porous film is 65 ° or less. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220151692-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021210498-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016087944-A |
priorityDate |
2011-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |