http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013045502-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-06 |
filingDate | 2011-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8eaeeff2e7252f1f31840490d8c0af48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f72447839937374bc31ae3eed8fbcfad http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_573e9fbed7533033672b66109b09f709 |
publicationDate | 2013-03-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013045502-A |
titleOfInvention | Composite polymer electrolyte membrane |
abstract | An electrolyte membrane relating to high proton conductivity and durability in order to achieve both a high level of proton conductivity and durability under low humidification conditions at a high temperature exceeding 90 ° C. and a relative humidity of 50% or less. Provided is an electrolyte membrane that suppresses changes in dry and wet dimensions and improves mechanical strength when wet. The composite polymer electrolyte membrane of the present invention is a composite polymer electrolyte membrane having a layer in which a space of a porous non-electrolyte material is filled with a polymer electrolyte material, When the cross section in the film thickness direction of the polymer electrolyte membrane is observed with an electron microscope, the following requirements are satisfied. (1) It has an island of a polymer electrolyte material having a thickness of 0.5 μm or less and a length of 2 μm or more. (2) A polyelectrolyte material island is connected to another polyelectrolyte material island. (3) It has an island of non-electrolyte material with a thickness of 0.1 μm to 2 μm and a length of 2 μm to 10 μm. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014186892-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020002505-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7107770-B2 |
priorityDate | 2011-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 56.