http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013041237-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F290-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-28 |
filingDate | 2012-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_968a9fb00a21712fff7f224cafa32388 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bf9043603bf321dae4bd0956ca5bf32c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0c6f087f3f211beeb1d52d01ee754d5f |
publicationDate | 2013-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013041237-A |
titleOfInvention | Photosensitive composition, photosensitive dry film, photosensitive laminate, flexible wiring board, method for manufacturing flexible wiring board, and method for forming permanent pattern |
abstract | A photosensitive composition, a photosensitive dry film, a photosensitive laminate, a flexible wiring board, a method for manufacturing a flexible wiring board, and a method for forming a permanent pattern, which are excellent in insulation, folding resistance, resolution and flame retardancy. Offer. SOLUTION: A binder resin, a polymerizable compound, a photopolymerization initiator and a thermal cross-linking agent are included, and the binder resin has an acid-modified ethylenically unsaturated group-containing polyurethane resin and a specific partial structure in a side chain. An acid-modified ethylenically unsaturated group-containing epoxy resin, the acid-modified ethylenically unsaturated group-containing polyurethane resin has a specific partial structure, and has a mass average molecular weight of 5,000 to 60,000, Photosensitive composition having a solid content acid value of 20 mgKOH / g to 120 mgKOH / g and an ethylenically unsaturated group equivalent of 0.5 mmol / g to 2.0 mmol / g, a photosensitive dry film using the same, and photosensitive property Laminated body, flexible wiring board, manufacturing method of flexible wiring board, and permanent pattern forming method. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7275898-B2 |
priorityDate | 2011-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |