Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G15-0233 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C35-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G15-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16C13-00 |
filingDate |
2012-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e09f66a336eece046f613d04697d6ab5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75f5ef039541d6bc8ca49896841569a5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fc8915aed4ecb8b2b84cd31eb52279f0 |
publicationDate |
2013-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2013033244-A |
titleOfInvention |
Charging member, method for manufacturing the same, and electrophotographic apparatus |
abstract |
The present invention provides a charging member that has sufficient flexibility to ensure a sufficient nip with a photoreceptor and can suppress the occurrence of a compression set. A charging member includes a support and an elastic layer, and the elastic layer has a surface MD-1 hardness of 55 to 85 ° and a pressing depth of 5 μm on the surface of the elastic layer. Universal hardness is 2.0-20.0 N / mm < 2 >. [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015127736-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10370525-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015034978-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9501032-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016206457-A |
priorityDate |
2011-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |