abstract |
An object of the present invention is to provide a carbon fiber reinforced resin composition excellent in mechanical properties, surface appearance, etc., and particularly excellent in tensile strength, flexural modulus, appearance / design, and dimensional stability. To do. A carbon fiber reinforced resin comprising 10 to 300 parts by weight of a carbon fiber (B) and 1 to 100 parts by weight of an amorphous resin (C) to 100 parts by weight of a thermoplastic polyamide resin (A). The glass transition temperature (Tg) of the amorphous resin (C) is preferably 100 ° C. or higher. [Selection figure] None |