abstract |
[PROBLEMS] To provide a thermoplastic resin composition excellent in oil resistance, particularly gasoline resistance, impact resistance, and conductivity. 30 to 80 parts by mass of polyamide, 20 to 70 parts by mass of a thermoplastic fluororesin (provided that the total of the polyamide and the thermoplastic fluororesin is 100 parts by mass), and carbon fiber, The content of the carbon fiber is 5 to 50 parts by mass with respect to 100 parts by mass in total of the polyamide and the thermoplastic fluororesin, and the tensile elongation of the thermoplastic fluororesin is 450% or more, and the tensile stress is A thermoplastic resin composition characterized by being 5 MPa or more. [Selection figure] None |