http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013001869-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e643df164d408263905077a4d3016558 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L99-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-00 |
filingDate | 2011-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e512fb8b6e0c7cdf4562d123a77f4dc8 |
publicationDate | 2013-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2013001869-A |
titleOfInvention | High damping composition |
abstract | PROBLEM TO BE SOLVED: To provide a high damping performance that can be sufficiently used as a vibration damper for buildings, etc., comprising a combination of S-IB diblock copolymer and S-IB-S triblock copolymer as a base polymer Disclosed is a novel high-damping composition capable of forming a high-damping member having excellent durability when repeatedly subjected to large elongation at break and large deformation. SOLUTION: The S-IB diblock copolymer and the S-IB-S triblock copolymer are mixed with 10 parts by mass or more of calcium carbonate, 5 parts by mass or more per 100 parts by mass of both block copolymers. 50 parts by mass or less of a tackifier and 5 parts by mass or more and 80 parts by mass or less of a paraffinic oil were blended. [Selection figure] None |
priorityDate | 2011-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |