http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012251042-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6765f97c95f6b26193d547fa6ddccf6b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G81-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G85-00 |
filingDate | 2011-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5716a4e15ae92f9786a78f591391fac0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46dca8582ad96fd4cfd876730b175382 |
publicationDate | 2012-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012251042-A |
titleOfInvention | Method for producing thermoplastic elastomer |
abstract | To provide a thermoplastic elastomer excellent in thermal stability, heat resistance and flexibility, a method for producing the same, and a molded body obtained by thermoforming the thermoplastic elastomer. At least a reactive group-containing elastomer, a cyclic polyester oligomer and a polyester polymerization catalyst are heated and mixed at a temperature of 120 to 300 ° C., and the mixture obtained in the step 1 is mixed with a phosphate ester compound and / or a hydrazide. A method for producing a thermoplastic elastomer, comprising a step 2 of mixing with an ester polymerization reaction inhibitor composed of a compound, a thermoplastic elastomer obtained by the method, and a molded article obtained by thermoforming the thermoplastic elastomer. [Selection figure] None |