http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012246417-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-02 |
filingDate | 2011-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e4c52a5cd22453ac1407267e51c8860 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e90b3cf5655a840a0187e2057b4dc96f |
publicationDate | 2012-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012246417-A |
titleOfInvention | Method for producing cellulose solution |
abstract | The present invention provides a method for producing a cellulose solution that has excellent pulp solubility and can reduce time and energy required for drying. A cellulose solution is produced by dissolving pulp in an ionic liquid. While making the moisture content of a pulp into 50 mass% or more, melt | dissolution to the ionic liquid of a pulp is performed under the heating of 70 degreeC or more. The pulp is preferably dissolved in the ionic liquid under a pressure lower than the vapor pressure of water in the mixture of the pulp and the ionic liquid at the temperature at the time of dissolution. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104878454-A |
priorityDate | 2011-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 365.