http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012226261-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c5520dd38cc403678d9f91e0b0ee95fb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 2011-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fca024fa7e2bde46732ac7911351c3b9 |
publicationDate | 2012-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012226261-A |
titleOfInvention | Toner and method for producing the same |
abstract | An object of the present invention is to provide a method for producing a melt-kneaded toner in which toner particles are less likely to block without decreasing hot offset resistance even when the rosin content is increased. Binder resin containing at least polyester resin A composed of benzenedicarboxylic acid and disproportionated rosin and glycerin and polyester resin B composed of at least benzenedicarboxylic acid and bisphenol A derivative; active silica fine particles; and carbon black The above-described problems are solved by the toner characterized by the above. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9068041-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2014170547-A1 |
priorityDate | 2011-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 149.