http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012211283-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K19-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 |
filingDate | 2011-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dbbd1590df4eecf62205d3f20094d3c0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f88df3925dd754edda1b8178beff8ef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81eacbeeb03d058be4bdb08477f29f2c |
publicationDate | 2012-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012211283-A |
titleOfInvention | Polymerizable liquid crystal composition |
abstract | PROBLEM TO BE SOLVED: To obtain a good free of cracks in the preparation of a patterned film using a combination of polymerization by ultraviolet irradiation and polymerization by heating in a polymerizable liquid crystal composition provided as an optical anisotropic material. It is to provide a material from which a film can be obtained. In a polymerizable liquid crystal composition containing a polymerizable liquid crystal compound, a photopolymerization initiator, and a thermal polymerization initiator, the 10-hour half-life temperature of the thermal polymerization initiator is 70 ° C or higher and 93 ° C or lower. Provided are a polymerizable liquid crystal composition and an optically anisotropic body obtained by curing the polymerizable liquid crystal composition. [Selection figure] None |
priorityDate | 2011-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 79.