http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012184332-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2ebdfc88803aa0e0bb776ddb9db35fda |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F297-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-6592 |
filingDate | 2011-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc5af0ee7fa06d2fd2c6d3151d68f0a0 |
publicationDate | 2012-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012184332-A |
titleOfInvention | Sealing material |
abstract | A low elution sealing material excellent in flexibility and heat resistance is provided. Propylene-ethylene component (A) satisfying the following (a1) to (a3): 30 to 70% by weight and a propylene-ethylene having an ethylene content of 3 to 25% by weight obtained using a metallocene catalyst It is based on the sealing material characterized by consisting of a polypropylene resin material containing 70-30 weight% of random copolymer components (B). (A1) Melting peak temperature (Tm) measured by DSC method is 125 to 155 ° C. (A2) The content of a comonomer selected from ethylene and an α-olefin having 4 or more carbon atoms is 0 to 5% by weight. (A3) Molecular weight distribution (Mw / Mn) measured by GPC method is 1.5-4 [Selection figure] None |