Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate |
2011-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bda58a3393c756078e5f64b22c3672ef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9ea66804e3bf4f7b633f5b4b3ee0d739 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cae07770cc5ff2ba1ea25c72eb37de9e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1dc435039130fe718b60269364f2b317 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c7ed712aa4b4bcd41866c9f0ee4208f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_583b1d705b089a17911ed421efe1f795 |
publicationDate |
2012-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2012177855-A |
titleOfInvention |
Resin for toner and toner |
abstract |
An object of the present invention is to provide a toner that has excellent high-temperature offset resistance and blocking resistance, and that suppresses the occurrence of fixing loss and has good low-temperature fixability. A resin for toner obtained by polymerizing a vinyl monomer in the presence of an unsaturated polyester resin, The unsaturated polyester resin has a first endothermic peak (P1) and a second endothermic peak (P2) in a DSC curve measured by a differential scanning calorimeter, and the first endothermic peak (P1). The peak temperature of the second endothermic peak (P2) is 80 ° C. or higher and 120 ° C. or lower. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10303072-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017203831-A |
priorityDate |
2011-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |