http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012176999-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J111-02 |
filingDate | 2011-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4695fd00077e9f6b4884f5f0969ae8e3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_472dd522af81962b6cd1d235f04849ab |
publicationDate | 2012-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012176999-A |
titleOfInvention | Water-based adhesive |
abstract | A water-based adhesive using a polyvinyl alcohol emulsified polychloroprene latex is improved in water-resistant adhesive strength. An aqueous adhesive comprising a polychloroprene latex obtained by emulsion polymerization in the presence of acetoacetylated polyvinyl alcohol and zinc oxide. The chloroprene polymer in the polychlorolatex is preferably a copolymer of chloroprene and a carboxyl group-containing vinyl monomer, and the toluene-insoluble content of the chloroprene polymer in the polychlorolatex is 10 to 90%. Is preferred. Moreover, it is preferable that the acetoacetylation degree of acetoacetylated polyvinyl alcohol is 0.05-15 mol%, and content of the zinc oxide in a water-system adhesive is a polychloroprene latex with respect to 100 mass parts in conversion of solid content. It is preferably 0.1 to 6.0 parts by mass in terms of solid content. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022216149-A1 |
priorityDate | 2011-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 192.