abstract |
[PROBLEMS] To improve the curing rate of benzoxazine. A thermosetting resin composition containing benzoxazine: 50 to 99% by mass and dicyclopentadiene-modified phenol: 50 to 1% by mass. Furthermore, a predetermined amount of novolac resin, silica, and the like can be included. [Selection figure] None |