http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012171799-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a55946e0f4dc12baad5eb7062ac05c7f |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B16-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B16-06 |
filingDate | 2011-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4657e69288adff96afecab728ca12813 |
publicationDate | 2012-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012171799-A |
titleOfInvention | INORGANIC PLATE AND METHOD FOR PRODUCING INORGANIC PLATE |
abstract | An inorganic plate excellent in wind pressure resistance and long-term durability, and a method for producing the same are provided. SOLUTION: A raw material mixture composed of cement, silicic acid-containing material, and organic fiber is extruded and contains cement and silicic acid-containing material in a mass ratio of 45:55 to 55:45. 3 to 8% by mass with respect to the total solid content, the specific gravity is 1.4 to 2.0, the moisture dimensional change rate at 80 ° C. for 10 days is 0.1% or less, and the water absorption dimensional change is 7 days. An inorganic plate having a rate of 0.1% or less, a 7-day dimensional change rate of 0.1% or less in an environment with a carbon dioxide concentration of 5%, and a flexural strength of 20 N / mm 2 or more. And the process of manufacturing the raw material mixture which consists of a cement, a silicic acid containing material, and an organic fiber, the process of extruding the obtained raw material mixture, manufacturing a mat, and autoclave curing at 140-200 degreeC. The manufacturing method of the inorganic board which consists of a process. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016160116-A |
priorityDate | 2011-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 46.