http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012158137-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_026917a1661e94c21035d1c5d1fa135e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-10 |
filingDate | 2011-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31f328c23036b92962f144aae69862c8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4d1ec687a98723cfb3350e5452d83b2f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86016793ba5e0de649d97f7e4077166d |
publicationDate | 2012-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012158137-A |
titleOfInvention | Paper sheet-containing composite material and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a composite material having high strength and a method capable of efficiently producing the composite material. SOLUTION: A composite material comprising at least a resin composition and a plurality of paper sheets, and a method for producing the composite material, the paper sheet The surface area of the composite material is 30 cm 2 or less, and a method for producing the same. It is preferable that the paper sheet contains fine plant fibers, and the width of the fine plant fibers is 2 nm to 1000 nm. The paper sheet preferably has an aspect ratio of 1.2 or more and is oriented in the composite material. [Selection] Figure 2 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114381960-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019505698-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016143645-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7107846-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11242652-B2 |
priorityDate | 2011-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 61.