http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012153550-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2dcebf5a7f7ddc3b081f70e8ce1c4097
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B7-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21C1-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F27D15-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B47-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21C5-28
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B5-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B5-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B5-00
filingDate 2011-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93dc4ac25d395f29724a81d793df124f
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e36353d88c76b3fc7d47f15df196b06d
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cebe3d82e9c31d4243206e6d8b9a7759
publicationDate 2012-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-2012153550-A
titleOfInvention Efficient method for recovering valuable metals from steelmaking slag
abstract An object of the present invention is to improve the recovery rate of iron-manganese oxide recovered from slag. A method of recovering valuable metals after performing a metal removal process for removing metal from a steelmaking slag containing a CaO—SiO 2 —P 2 O 5 phase and a (Fe, Mn) Ox phase. Thus, the basicity becomes 1.5 to 2.5 within a temperature range of 1250 to 1400 ° C. for steelmaking slag having a basicity of less than 1.5 after the treatment or steelmaking slag having a basicity of more than 2.5. The steelmaking slag that has been subjected to the reforming process and subjected to the metal removal process and the reforming process is pulverized so that the representative particle size after pulverization is 50 μm or less, and the slag after the pulverization process is roughened. In the classification process of classifying into fine particles and fine particles, the ratio of the representative particle size of the coarse particles to the representative particle size of the fine particles is processed to be 2.5 times or more, and the coarse particles are recovered after the classification treatment. is there. [Selection] Figure 1
priorityDate 2011-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011236115-A
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID165915
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419520343
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID160959
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451845207
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID123290
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451276627

Total number of triples: 27.