http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012136715-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 |
filingDate | 2012-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8746d7491d328fa9f540c600eae31d58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ddf3faf10f8f5bee72067e5ed352c60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_90c96eac185abd1a9f6fa3c6890c06ce |
publicationDate | 2012-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012136715-A |
titleOfInvention | Resin composition and molded article comprising the same |
abstract | An environmentally low-load resin composition having excellent strength, impact resistance, heat resistance and molding processability and capable of reducing CO 2 emission during production is obtained. [Solution] A resin composition comprising (A) a styrene resin, (B) a graft polymer, (C) an aliphatic polyester, and (D) an impact modifier, preferably (A) a styrene resin, and (B) a graft. The total amount of (C) aliphatic polyester and (D) impact modifier is 30 to 60% by weight of the styrene resin, and (B) the graft polymer is added. A resin composition having 10 to 50% by weight, (C) an addition amount of an aliphatic polyester of 60 to 10% by weight, and (D) an addition amount of an impact resistance improver of 2 to 20% by weight. [Selection figure] None |
priorityDate | 2005-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |