http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012122132-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e3b0a3dbf8d6c9712d86ea1383fd5327 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F2999-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F3-1007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C32-0021 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F3-02 |
filingDate | 2011-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7180593bfe7188e3cecdfc04cdc0703d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7642a3bb0d8f6a490db1d34ccf6da4a8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da40c8603259fb340d5ed51b789dbdd0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_30a3bcecca04e051e549b4caf5f650c8 |
publicationDate | 2012-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012122132-A |
titleOfInvention | Clay-like composition for forming sintered body, powder for clay-like composition for forming sintered body, method for producing clay-like composition for forming sintered body, copper sintered body, and method for producing copper sintered body |
abstract | A clay-like composition for forming a sintered body (copper clay) that can be fired in a non-oxidizing atmosphere without performing a calcination step in an air atmosphere, and a clay-like composition for forming a sintered body Provided are a powder for a composition, a method for producing a clay-like composition for forming a sintered body, a copper sintered body, and a method for producing a copper sintered body. A powder component containing a copper-containing metal powder containing copper and a copper-containing oxide powder containing copper, a binder, and water, and the amount of oxygen contained in the powder component is 4% by mass. It is characterized by being in the range of 8 mass% or less. Furthermore, the sinterability of a copper sintered compact improves because content of Fe shall be 1000 ppm or less. [Selection figure] None |