Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9df90d7822cc480ce12c480f4089e229 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5c039f60302b61e712887aa2267ecbe |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-5825 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B35-12 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B35-04 |
filingDate |
2010-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b05228f48d82b06de85adc2c4d23a5d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_41a72847a81493295bf2b5532b0bf6a5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c771b908ac4b8e606f98c3e0f55a86f9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79b141f55718f429a6b56184197a412f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3aa389d39ce73df041e05b584259aab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_512bcb694daa18a20a28401f82425b76 |
publicationDate |
2012-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2012104240-A |
titleOfInvention |
Method for producing lithium borate compound |
abstract |
A lithium borate-based material useful as a positive electrode material for a lithium ion secondary battery is provided with a method capable of producing a material having excellent performance with improved cycle characteristics, capacity, and the like near room temperature. The method for producing a lithium borate compound of the present invention is at least one selected from the group consisting of a lithium-containing molten salt raw material containing at least lithium nitrate, and pure iron, pure manganese, and a compound containing iron and / or manganese. In a molten salt of the lithium-containing molten salt raw material having a melting point of 900 ° C. or lower and a melting point of the lithium-containing molten salt raw material in a mixed gas atmosphere containing carbon dioxide and a reducing gas. React with. [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013230273-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013230272-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013230271-A |
priorityDate |
2010-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |