Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_52da78de6e863642797915d12dd3bbb9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B24-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E21D11-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-10 |
filingDate |
2010-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_76ab6889b64afe28e6e58a80e75dce3a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9cfbbe33b65fbb22660eb7831c1faa34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02f6cd507a0c0ebcd2967fda9dc7fc96 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e02832058fe0d37352adcbc1ca08269f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d692bef362470dcad1c8cf1395244cd8 |
publicationDate |
2012-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2012097497-A |
titleOfInvention |
Quick setting cement concrete lining method |
abstract |
PROBLEM TO BE SOLVED: To provide a method for lining quick-setting cement concrete that can increase the filling property with less leakage from a mold. A compressed air supply pipe 3 for adding water is connected to a powder quick setting agent supply pipe 1 for pneumatically feeding a powder quick setting agent containing calcium aluminates, gypsum and a setting retarder. The water is pressed into the compressed air supply pipe 3 through which compressed air of 1 to 5 m 3 / min flows at least 0.1 MPa higher than the pressure feeding pressure of the powder quick setting agent, and then the powder quick setting agent Is mixed into a slurry to obtain a quick setting slurry, and this quick setting slurry is added to and mixed with cement concrete having a slump flow of 30 to 70 cm through a mixing pipe 6 to form a quick setting cement concrete. The lining method is configured such that the mold is filled and covered from the bent tube nozzle 8 having a bending angle of 20 to 150 degrees via the second transport pipe 7. [Selection] Figure 2 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109404014-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109356619-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109322681-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2016208277-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2022108336-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016208277-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103291324-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014190014-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7293264-B2 |
priorityDate |
2010-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |