Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-48 |
filingDate |
2010-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c87ba06fd92698fe1730d3752579b8bd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_beb4f764d6f33c1787c88edf44a1d929 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c04e07540764709b5dd34a4661a1653 |
publicationDate |
2012-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2012096977-A |
titleOfInvention |
Colored translucent zirconia sintered body, method for producing the same, and use thereof |
abstract |
【Task】 A colored translucent zirconia sintered body that has a clear color tone and high transparency as a fine member, is excellent in both design and aesthetics, and can easily obtain an arbitrary shape. A sintered body and a method for producing the same are provided. [Solution] Colored translucency characterized by containing yttria in an amount of 6 mol% to 15 mol%, titania in an amount of 3 mol% to 20 mol%, an lanthanoid rare earth element in an oxide equivalent of at least 4 mol%, and a porosity of at most 1000 ppm. Zirconia sintered body. The average crystal grain size is preferably at most 60 μm. [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018002495-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018002528-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110418773-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7192908-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018002527-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021113152-A |
priorityDate |
2010-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |