http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012092313-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-215 |
filingDate | 2011-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_91570144b7e8bffb702750ed1b37f353 |
publicationDate | 2012-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012092313-A |
titleOfInvention | Method for producing slurry composition |
abstract | The present invention provides a method for producing a slurry composition capable of realizing excellent dispersibility even with a small amount of solvent by a simple process. Moreover, the slurry composition manufactured using the manufacturing method of this slurry composition is provided. A method for producing a slurry composition containing an inorganic powder, a polyvinyl acetal resin and an organic solvent, wherein the inorganic powder, the polyvinyl acetal resin (A) and an organic solvent for inorganic dispersion are added and mixed to form an inorganic dispersion. A step of adding a polyvinyl acetal resin (B) and an organic solvent for a resin solution to prepare a resin solution, and a step of adding a resin solution to the inorganic dispersion, and the polyvinyl acetal The resin (A) has a degree of polymerization of 20 to 600 and a hydroxyl group amount of 37.5 to 47 mol%. The polyvinyl acetal resin (B) has a polymerization degree of 800 to 4200 and a hydroxyl group amount of 28 to 42. In the step of preparing the inorganic dispersion, the polyvinyl acetal resin (A) is added in an amount of 0.1 to 20 parts by weight based on 100 parts by weight of the inorganic powder. Method for producing a slurry composition to be added quantity unit. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014072103-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013035694-A |
priorityDate | 2010-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 82.