Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f4d9d138d23c7ca8bfae3daf28b4eba0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M2-16 |
filingDate |
2011-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dc17adaa72ad84c575989e9209aca11 |
publicationDate |
2012-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2012092302-A |
titleOfInvention |
Porous film, battery separator and battery |
abstract |
【Task】 It is an object of the present invention to provide a porous film having an excellent air permeability that contributes to electrical performance and having an important shutdown characteristic in terms of ensuring safety. [Solution] The main component of the present invention is a poly-4-methyl-1-pentene polymer resin composition in which at least one peak loss tangent temperature measured by dynamic viscoelasticity measurement at a frequency of 10 Hz is between −100 to 20 ° C. A component in which the poly-4-methyl-1-pentene polymer resin composition is a poly-4-methyl-1-pentene polymer, and as a soft component, a vinyl aromatic compound and A porous film characterized in that it is a resin composition comprising a copolymer with a conjugated diene or a component that is a hydrogenated derivative thereof, and is stretched in at least one direction. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115298279-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3766927-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11491760-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014004771-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019176743-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020096061-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017222823-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2021046731-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014233897-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019176743-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103601990-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016203621-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021028396-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013035622-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2020096061-A1 |
priorityDate |
2010-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |