http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012082243-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_47cc435e1d443f13180f7766df104d9d |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07K14-435 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 |
filingDate | 2010-10-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b69b63f4f9948b9bb315fd68bc458c31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a08758e8ba7e8eade2eb423ca13a4958 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bef3e6f7e04d5332948eccf0cb1a4b97 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b0c1adb31e1b8feef49c4e93d1ecea3 |
publicationDate | 2012-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012082243-A |
titleOfInvention | Method for producing silk fibroin porous material |
abstract | The present invention easily adjusts the structure of the porous body such as the pore diameter and the number of pores and the strength of the porous body, and has a porous body having a structure with a smaller pore diameter and higher strength. To provide a method for producing a porous body having A silk fibroin solution obtained by adding an acidic amino acid to a silk fibroin aqueous solution is allowed to stand for 10 hours or more at a temperature at which the solution does not solidify, and the silk fibroin solution after standing is frozen and then thawed. A method for producing a silk fibroin porous body. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109880154-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012082246-A |
priorityDate | 2010-10-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 27.