Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-414 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2431-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2423-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2400-143 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10871 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10788 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2367-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10036 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10697 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10862 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10005 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-12 |
filingDate |
2010-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_240ef4deeb94cd045092588402353980 |
publicationDate |
2012-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2012066984-A |
titleOfInvention |
Laminated glass manufacturing method |
abstract |
A method of manufacturing a laminated glass using an intermediate film containing EVA as a main component by using a process including pressurization by a nip roll, which can satisfactorily remove bubbles in the laminated glass. I will provide a. The composition comprises an ethylene-vinyl acetate copolymer and a crosslinking agent, and has a melt viscosity of 2 × 10 5 Pa · s or less at a temperature of 70 ° C., and an arithmetic average roughness Ra (at least one surface) JIS-B0601 (2001)) is 5 to 20 μm, and an intermediate film 12 provided with one or more ethylene-vinyl acetate copolymer layers having an average thickness of 0.5 mm or more is composed of two or more glasses. The process of obtaining the laminated body 20 by sandwiching between the plates, the pressure-bonding process in which the laminated body 20 is heated and then pressed by using the nip roll 34, and the laminated body 20 ′ is further heated after the pressure-bonding process. A method for producing a laminated glass comprising the step of cross-linking and integrating. [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3015522-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015059052-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014208756-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015196612-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017006982-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020055746-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104118186-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017088487-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105489706-A |
priorityDate |
2010-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |