http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012066586-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f4d9d138d23c7ca8bfae3daf28b4eba0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 |
filingDate | 2011-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_300dbe193f9ca3d2b7630ee1dc0db18b |
publicationDate | 2012-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012066586-A |
titleOfInvention | Polyester film for simultaneous transfer of molding |
abstract | A biaxially stretched polyester film having sufficient moldability, heat resistance and transferability is provided. [MEANS FOR SOLVING PROBLEMS] At least one side of a B layer comprising a polyester containing at least one copolymer component other than the main component and having a main component content of 90 mol% or less has a main component content. A film having a structure in which an A layer made of polyester of 80 mol% or more is laminated, wherein the melting point (TmA) of the A layer is 190 to 260 ° C, and the melting point (TmB) of the B layer is 180 to 230 ° C. The difference between the melting points (TmA-TmB) is 5 ° C. or more, and the storage elastic modulus E ′ of the film is in the range of 810 to 1100 MPa at 80 ° C. and 10 to 80 MPa at 160 ° C. Polyester film for simultaneous transfer of molding. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013226723-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2017130952-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017130952-A1 |
priorityDate | 2011-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 39.