http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012056998-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-337 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 |
filingDate | 2010-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eee95d0e4a3019825656c08e77a11efc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_48ab527e0131defa9278866bf31dbf23 |
publicationDate | 2012-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012056998-A |
titleOfInvention | Dispersion and thermal recording material |
abstract | PROBLEM TO BE SOLVED: To provide a heat-sensitive recording material excellent in color development sensitivity and background whiteness by preparing a dispersion liquid having excellent dispersion efficiency, little liquid fog, and excellent dispersion stability and storage stability. SOLUTION: It has a group represented by the following general formula (I) at its end, a modification amount S is 0.1 to 3.0 mol%, a viscosity average polymerization degree P is 100 to 1000, and A dispersion containing a vinyl alcohol polymer having a saponification degree of 40 to 99.9 mol%. [Chemical 1] (In the formula, R represents a hydrogen atom or an OM group, and M represents a hydrogen atom, an alkali metal atom, a 1/2 alkaline earth metal atom, or an ammonium group.) [Selection figure] None |