http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012056218-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-337 |
filingDate | 2010-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_21ff45f1a66214cc5b8d5937cd387772 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7e97c1e3e3678c2865b024561af48e72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a82fd19b3e89d3a3590c0467d1a78580 |
publicationDate | 2012-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012056218-A |
titleOfInvention | Resin for thermal paper protective layer and thermal recording material using the same |
abstract | [PROBLEMS] To improve the durability (plasticizer resistance, water resistance, heat resistance) of recording layers and recorded images of heat-sensitive recording materials, and to improve scratches and cracks during processing, and the accompanying peeling of the protective layer. It is to provide a heat-sensitive recording paper protective layer resin and a heat-sensitive recording material. A resin for a heat-sensitive recording paper protective layer contains a resin emulsion (C) comprising a polyvinyl alcohol (A) and a hydrophobic copolymer (B) having at least a cyano group-containing vinyl monomer (b1), A resin for a thermal recording paper protective layer in which the ratio of (A) to (B) is 20 to 90 parts by weight of (A) with respect to 100 parts by weight of (B). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016107608-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114481698-A |
priorityDate | 2010-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 50.