http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012052279-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M101-40 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-41 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-55 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-477 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-463 |
filingDate | 2011-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36f4976dddcb6c2d7e18912bba84e094 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bbfb01d9c26c33242b8881abea537ebb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b560ffcd3883e3e40bd8db336696c7f1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_89061d8a34a8aa197294aebc3ff305c1 |
publicationDate | 2012-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012052279-A |
titleOfInvention | Method for producing carbon fiber coated with sizing agent |
abstract | Disclosed is a method for producing carbon fiber coated with a sizing agent, which has excellent adhesion between carbon fiber and a matrix resin and is excellent in high-order processability. As the component (A), a bifunctional or higher functional epoxy compound (A1) and / or a monofunctional or higher functional epoxy group having a hydroxyl group, an amide group, an imide group, a urethane group, a urea group, a sulfonyl group, And 100 parts by mass of the epoxy compound (A2) having at least one functional group selected from sulfo groups, 0.1 to 25 mass of a quaternary ammonium salt having a cation moiety having a specific structure as the component (B) A method for producing sizing agent-coated carbon fiber, in which a sizing agent obtained by blending parts is applied to carbon fiber and heat-treated at a temperature range of 160 to 260 ° C. for 30 to 600 seconds. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013249562-A |
priorityDate | 2010-08-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 472.