http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012051970-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c389d310f52125a947b3408cb0cf3283 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C5-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C19-28 |
filingDate | 2010-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53ed0843e8e9c2f027c3da12774251a4 |
publicationDate | 2012-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012051970-A |
titleOfInvention | Process for producing modified diene rubber polymer |
abstract | To improve air permeation resistance. After irradiating an uncured diene rubber polymer made of natural rubber and / or isoprene rubber with an electron beam, it has a carbon-carbon double bond in the molecule, and has a hydroxyl group, a nitrile group and a halogen atom. A modified diene rubber polymer is prepared by applying a compound having at least one functional group selected from the group consisting of the above to the diene rubber polymer that has been irradiated with electrons, thereby reacting the compound with the diene rubber polymer. Get. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020255823-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020095891-A1 |
priorityDate | 2010-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 66.