http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012046615-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ead90443277482e25bf91bfddef2b5a7 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G59-62 |
filingDate | 2010-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8896389057e9be1306a662309cac1896 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31ac515fbdccd590941928ff4cd7b0da |
publicationDate | 2012-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012046615-A |
titleOfInvention | Epoxy resin, production method thereof, epoxy resin composition and cured product |
abstract | [PROBLEMS] To provide an epoxy resin that gives a cured product excellent in high thermal decomposition stability, high heat resistance, low thermal expansion, flame retardancy, low hygroscopicity, its production method, an epoxy resin composition using this epoxy resin, and its Provide a cured product. An epoxy resin obtained by reacting a phenolic resin represented by the following general formula (2) with epichlorohydrin, and an epoxy resin composition containing the epoxy resin and a curing agent as essential components, and the epoxy resin It is a cured product obtained by curing the composition. In the formula, m represents a number from 1 to 15. [Selection figure] None |
priorityDate | 2010-08-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |