http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012013972-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_50f9d52c04326083376d1a1f199b34cc |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2010-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3fd271dde58eefebdcd54f8f5b15e00f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e758c0b06e3eb2dde515304d51d0ed3 |
publicationDate | 2012-01-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012013972-A |
titleOfInvention | Low temperature fixability and blocking resistance improver for toner |
abstract | 【Task】 A binder resin containing a polyglycerin fatty acid ester that improves the low-temperature fixability, blocking resistance, and printing durability of the toner, and improves the low-temperature fixing property, blocking resistance, and printing durability, and a binder resin; An object of the present invention is to provide a toner excellent in low-temperature fixability, hot offset resistance, blocking resistance, and printing durability. [Solution] A polyglycerin having a total triglycerin concentration and a tetraglycerin concentration of 50% by weight or more and a concentration of each of triglycerin and tetraglycerin in the range of 10% by weight to 70% by weight, and a carbon number of 16-22 By blending the toner with a polyglycerin fatty acid ester composed of a saturated fatty acid, low-temperature fixability, hot offset resistance, blocking resistance, and printing durability of the toner are improved. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014109704-A |
priorityDate | 2010-07-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 64.