http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012012747-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5d123e76a98aad8db100e9f8c62e0648 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F8-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02J1-00 |
filingDate | 2010-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cb220c8e7ef5876feba86f076d700569 |
publicationDate | 2012-01-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2012012747-A |
titleOfInvention | 制 Antistatic polyester blended yarn with excellent recovery |
abstract | [Problem] To provide a polyester mixed yarn that maintains the soft texture, heat retention, water absorption, moisture absorption, and other properties of a conventional ultra-fine polyester yarn, and is excellent in antistatic properties and wrinkle recovery properties. is there. SOLUTION: A blended yarn composed of two types of polyester multifibers having different elongation, elastic recovery rate, elongation rigidity rate, and boiling water shrinkage rate, and one component polyester multifiber is a core-sheath type composite fiber, A mixed yarn obtained by entanglement treatment with another polyester multi-fiber after the relaxation heat treatment, wherein the core component contains a specific antistatic agent and is obtained at a specific range of spinning speed. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017008190-A |
priorityDate | 2010-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 82.