Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c85c5c0d468cc3c8085c4a34b25700ff |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J157-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D4-00 |
filingDate |
2011-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1791da09b580d7817a35be76ab6117c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9ab8d740286b18fe2a48ceded176a96b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ad839aa64691d0cb41f2663bf27bdbbe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6056b0268b559e85001637448d37c784 |
publicationDate |
2012-01-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2012007174-A |
titleOfInvention |
Method for preparing a pressure sensitive adhesive |
abstract |
The present invention provides a pressure-sensitive adhesive preparation method in which defects of the conventional pressure-sensitive adhesive preparation methods are improved. (I) providing an essentially solvent-free mixture comprising one or more radically polymerizable monomers having one ethylenically unsaturated group and at least one radical polymerization initiator; (ii) ) Partially polymerize the mixture to a Brookfield viscosity of 1,000-125,000 mPa · s at 20 ° C. and 30-60 wt% monomer to polymer relative to the initial mass of monomer before polymerization. Providing a partially polymerized mixture exhibiting conversion, (iii) adding one or more radical radiation polymerization initiators to the partially polymerized mixture to provide a radiation curable precursor, (iv) Applying the radiation curable precursor to a substrate; and (v) subjecting the radiation curable precursor to actinic radiation to further polymerize the radiation curable precursor. Comprising the step of providing the pressure sensitive adhesive. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020109138-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020141606-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7244278-B2 |
priorityDate |
2003-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |