http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011256237-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5ac17835c97e6c72213815ca74845386 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 |
filingDate | 2010-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3ae6385238834384e50eaf9a3e5bf4b5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0049bab938514a5453bef0bc4650a59 |
publicationDate | 2011-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011256237-A |
titleOfInvention | Coating liquid, coated material, and manufacturing method of coated material |
abstract | [PROBLEMS] To provide a coating liquid and a coating material that have excellent gold luster and can adjust a delicate hue such as reddish, greenish, yellowish, or bluish, and a manufacturing cost without requiring a complicated process. It also provides an advantageous method for producing a coated product. The present invention provides a coating liquid containing gold nanoparticles [A] and a silane coupling agent [B], wherein the silane coupling agent [B] contains a diamino structure, a mercapto group, and a sulfide group. And the content of the silane coupling agent [B] is 1 with respect to 100 parts by mass (in terms of metal) of the gold nanoparticle [A]. It is a coating liquid characterized by being no less than 20 parts by mass. The constituent metal of the gold nanoparticle [A] is preferably gold or an alloy containing gold. [Selection figure] None |