http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011253007-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-10 |
filingDate | 2010-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d4c9ad50ab9a8ea61a78d90d1787512e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c403e1ec0874e8953c9c403767382f2 |
publicationDate | 2011-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011253007-A |
titleOfInvention | Image forming method using two-component developer |
abstract | The present invention maintains a good charge rising property and a good charge amount level of a developer even when different toners are replenished, and fog, toner scattering, in all environments including high temperature and high humidity and low temperature and low humidity. It is an object of the present invention to provide an image forming method that does not cause paper contamination. Forming an electrostatic latent image on an image bearing member; developing the electrostatic latent image with a two-component developer including an electrostatic charge image developing toner and a carrier; and forming a toner image; An image forming method including a step of sequentially supplying replenishment toner, When the toner concentration in the two-component developer is 6 wt%, the fluidity of the two-component developer is 100 seconds / 50 g or more, and as an external additive for the toner filled in the developing cartridge and / or the replenishment toner. A positively charged metal oxide particle having a BET specific surface area of 100 m 2 / g or more and two negatively charged metal oxide particles having a BET specific surface area of 110 m 2 / g or less and different BET specific surface areas. This is solved by a characteristic image forming method. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015158590-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9229347-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015098889-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014071418-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015143851-A |
priorityDate | 2010-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 146.