http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011213809-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_75249adb90a4cfa442d4751eea6ee07e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D125-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 |
filingDate | 2010-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_39e182aebdf2de96a62a912638ddaaf7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dfdba77529143bd655f86d89e5ac7046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d8690edaf6f0c5971961fcdb0fce033 |
publicationDate | 2011-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011213809-A |
titleOfInvention | Coating composition and application method thereof |
abstract | An object of the present invention is to provide a storage product that has good storage stability, does not cause unstable jetting when it is pressurized by electric driving and jets fine droplets, is fast in drying, has no repelling or blurring, and has a favorable quality. To provide a coating composition excellent in expression. In a coating composition containing a pigment, a resin component, a solvent, and water, having a viscosity at 20 ° C. of 30 mPa · s or less and a surface tension of 21 to 34 mN / m, The resin component is 1 to 20% by weight in the coating composition, Coating composition in which the solvent ratio in the coating composition is 5 to 40% by weight, contains at least one solvent (a) as a solvent, and the solvent (a) contains 5 to 100% by weight in the total solvent: Solvent (a) A droplet of the solvent aqueous solution having a contact angle at 20 ° C. of 20 ° C. or less of 10% by weight after 10 seconds when dropped onto a plastic substrate having a contact angle with water at 85 ° C. of 85 to 95 ° is added to the plastic substrate. A solvent having a contact angle of 20 ° or less at 20 ° C. after 10 seconds when dropped on a material. [Selection figure] None |
priorityDate | 2010-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |