http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011200791-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e64079869bbb0e5ffa9fc45afaab5395 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 |
filingDate | 2010-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_037a461f36d6d7ef22ef0a14ff24cf9e |
publicationDate | 2011-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011200791-A |
titleOfInvention | Laminate coating formation method |
abstract | [PROBLEMS] To achieve energy saving while suppressing an increase in the amount of solvent used in a base paint while obtaining good paint finish in forming a multilayer paint film. A solvent-type base paint containing a polyol resin and a curing agent is applied on an electrodeposition coating film 2 of an object to be coated 1, and a two-component urethane clear paint containing a polyol resin and an isocyanate is applied thereon. In a multilayer coating film forming method in which a base coating film 3 and a clear coating film 4 are formed by wet-on-wetting, and the base coating film 3 and the clear coating film 4 are simultaneously baked and cured, , One having 3 or more branches extending radially from the center of the molecule and having a mass average molecular weight of 6000 or more is used. [Selection] Figure 1 |
priorityDate | 2010-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |