http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011190960-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b3a237e06cefa8a053ea8e184cd010c3 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F25D3-00 |
filingDate | 2010-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_04918d1284753a195d44e6cdb084dffe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_85524ed56fda2fd26ebabc4e75b58f4a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_014826ef7ce20b0b376c745a3813ad1e |
publicationDate | 2011-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011190960-A |
titleOfInvention | Resin material for regenerator container and regenerator container |
abstract | The present invention provides a resin material for a regenerator container capable of improving thermal conductivity and durability against repeated freezing and thawing. A resin material for a regenerator container contains a high-density polyethylene resin having a melt flow rate of 0.01 to 10 g / 10 min as defined in (A) JISK6922-1 as a base material, and further (B ) An ethylene-α-olefin copolymer and (C) a spherical filler. [Selection figure] None |