http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011190558-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4a60326471cf8e73187625e940919ea0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H17-67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-38 |
filingDate | 2010-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1c96f8febe42ec4d8c4463cc697fca1 |
publicationDate | 2011-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011190558-A |
titleOfInvention | Coated paper |
abstract | [PROBLEMS] To suppress generation of wrinkles even when printing is performed using a high-speed rotary offset printing machine, particularly a high-speed rotary offset printing machine having a printing speed of 1000 rpm or higher, and has high white paper gloss and printing gloss, and high surface strength. Therefore, it provides a coated paper for printing that looks good and has an excellent finish. As a pigment in the coating layer, pigment particles having a particle diameter of 2 μm or more are 5% or less of the total pigment particles, and the coating layer has a butadiene component of 50% by mass or more as an adhesive. -4-7 mass parts of butadiene latex are contained with respect to 100 mass parts of said pigments. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012214960-A |
priorityDate | 2010-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 35.