http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011189871-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c06ff00cc23d0d0c48233a171dccb984 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60H1-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L57-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60R13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-00 |
filingDate | 2010-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b57984e92ba4d53ea19062f0364edba1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_55f52da606b589c886c6ddf99f5ff227 |
publicationDate | 2011-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011189871-A |
titleOfInvention | Automotive interior parts with reduced squeaking noise |
abstract | An interior of an automobile in which the squeaking noise generated when the members rub against each other is remarkably reduced, and the effect of reducing the squeaking noise is maintained without being deteriorated even when left under a high temperature for a long time. Provide parts. A thermoplastic resin composition comprising a rubber-reinforced vinyl resin obtained by polymerizing a vinyl monomer in the presence of an ethylene / α-olefin rubber polymer, the ethylene -From the group of the following Y1-Y4, and the molded product of the thermoplastic resin composition whose content of (alpha) -olefin type rubber-like polymer is 5-30 mass% by making the whole thermoplastic resin composition into 100 mass% It consists of a molded product of a selected thermoplastic resin. Y1: Polycarbonate / rubber reinforced styrene resin alloy with HDT of 85 ° C or higher, Y2: Styrenic resin with HDT of 85 ° C or higher (excluding Y1), Y3: Polyolefin resin with HDT of 85 ° C or higher, and Y4: Methacrylic resin having an HDT of 85 ° C. or higher. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015120937-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015157950-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015134879-A |
priorityDate | 2010-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 243.