http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011174209-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-485 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-4309 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F8-10 |
filingDate | 2010-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4540100a10345b91a5ef7ab7f70e93d0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_18f210466757d297e3bb88bfea164c07 |
publicationDate | 2011-09-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2011174209-A |
titleOfInvention | Flame retardant composite fiber |
abstract | Disclosed is a composite fiber that has high adhesion during wet heat treatment and is flame retardant without using harmful components. In a composite fiber formed by melt-spinning an ethylene-vinyl alcohol copolymer (A) having an ethylene content of 10 to 60 mol% and another thermoplastic polymer (B), At least part of the surface of the composite fiber is composed of an ethylene-vinyl alcohol copolymer, and 0.005 to 1.0 mass of a boron-based flame retardant is added to the ethylene-vinyl alcohol copolymer (A). % (Vs. A) plus composite fiber formed by melt composite spinning. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017043726-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015045982-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015045982-A1 |
priorityDate | 2010-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 125.